Author Topic: Rhydrating bows  (Read 1777 times)

0 Members and 1 Guest are viewing this topic.

Offline Lee Lobbestael

  • Member
  • Posts: 465
Rhydrating bows
« on: November 08, 2010, 08:07:58 pm »
How long do you guys let bows sit to rehydrate before bending them again after you heat treat them or put heat bends into them? I usually wait a week but do you think I could get away with three or four days?

Offline sailordad

  • Member
  • Posts: 5,045
Re: Rhydrating bows
« Reply #1 on: November 08, 2010, 08:14:26 pm »
what little heat work ive done,i let them sit a week
also depends on the the rh is at the time
a little longer is better,than not long enough  ;)
i always wanted a harley,untill it became the "thing to ride"
i ride because i love to,not to be part of the crowd

Offline mullet

  • Global Moderator
  • Member
  • Posts: 22,911
  • Eddie Parker
Re: Rhydrating bows
« Reply #2 on: November 08, 2010, 10:34:23 pm »
 It depends on the humidity and where you store them. If it's anytime but winter here I'll work on it the next day.
Lakeland, Florida
 If you have to pull the trigger, is it really archery?

Offline Del the cat

  • Member
  • Posts: 8,322
    • Derek Hutchison Native Wood Self Bows
Re: Rhydrating bows
« Reply #3 on: November 09, 2010, 10:31:46 am »
I'm pretty new to heat treating, just doing Hazel bow, it's had 4 heat treatments during tillering, I've given it 2-3 days minimum after each.
I think it needed longest after the first, the later ones have been more of a top up and seemed to get going quicker.
Mind it's been humid here, if it's not raining then it just about to, or it's just stopped. Getting chilly too.
Del