So I am making a bow out of yew and I am flipping the tips. I am wondering how long to boil or steam? And which is better? Thanks for any input.
"Judge a man by his questions, not his answers" ~Anonymous

   "The person who says it cannot be done should not interrupt the person who is doing it." ~Chinese Proverb

Offline adb

  • Member
  • Posts: 5,339
Re: Yew recurve ??'s
« Reply #1 on: November 18, 2013, 09:26:15 pm »
Yew bends like cheese. I've used mostly dry heat, but steam is good too. 30-40 mins is plenty.

blackhawk

  • Guest
Re: Yew recurve ??'s
« Reply #2 on: November 18, 2013, 09:29:02 pm »
How far of an angle are you bending them? For contact recurve tips use steam...if your just flipping them a little bit dry heat will get you there....when yew gets hot enough it bends like a wet cooked noodle...

Offline wood_bandit 99

  • Member
  • Posts: 197
  • Shoot straight my friends!!   55#@26"
Re: Yew recurve ??'s
« Reply #3 on: November 19, 2013, 12:00:48 am »
I would like to make it either. It will most likely make a flipped tips though. I tried dry heat bending some major deflex out of it. It worked, but not as good as I would have liked (obviously osage is the only wood I've worked with ;D) I may try dry heat. I was bending quite a bit of wood last time. If it doesn't how long to boil/steam? I have one vote for around 40 min?
"Judge a man by his questions, not his answers" ~Anonymous

   "The person who says it cannot be done should not interrupt the person who is doing it." ~Chinese Proverb

mikekeswick

  • Guest
Re: Yew recurve ??'s
« Reply #4 on: November 19, 2013, 04:14:28 am »
The rule of thumb is 30 mins per 1/2 inch thickness.