Author Topic: Cutlers Resin - The Old Term for Pine Pitch Glue  (Read 11973 times)

0 Members and 1 Guest are viewing this topic.

Offline JackCrafty

  • Global Moderator
  • Member
  • Posts: 5,628
  • Sorry Officer, I was just gathering "materials".
Cutlers Resin - The Old Term for Pine Pitch Glue
« on: November 29, 2011, 04:58:40 pm »
Just thought I'd share this one.  From wikipedia:

Cutler's Resin is a synthetic resin made of pine pitch, beeswax, and sawdust or carnauba wax used for centuries (to today) to attach knife handles. It is used as both an adhesive and for waterproofing. The word cutler means "one who makes knives". http://en.wikipedia.org/wiki/Cutler's_resin

Here's a web page with lots of links:

http://leatherworker.net/forum/index.php?showtopic=23929
Any critter tastes good with enough butter on it.

Patrick Blank
Midland, Texas
Youtube: JackCrafty, Allergic Hobbit, Patrick Blank

Where's Rock? Public Waterways, Road Cuts, Landscape Supply, Knap-Ins.
How to Cook It?  200° for 24hrs then 275° to 500° for 4hrs (depending on type), Cool for 12hr

Offline mullet

  • Global Moderator
  • Member
  • Posts: 22,911
  • Eddie Parker
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #1 on: November 29, 2011, 07:15:53 pm »
Wow, that's interesting.
Lakeland, Florida
 If you have to pull the trigger, is it really archery?

Offline JackCrafty

  • Global Moderator
  • Member
  • Posts: 5,628
  • Sorry Officer, I was just gathering "materials".
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #2 on: November 29, 2011, 07:44:18 pm »
Eddie, it would have saved us all a lot of trouble if we knew about this stuff sooner.  From now on, I'm just going to tell the newbies to look up "cutlers resin" when they ask me about pitch glue.

 ::)
Any critter tastes good with enough butter on it.

Patrick Blank
Midland, Texas
Youtube: JackCrafty, Allergic Hobbit, Patrick Blank

Where's Rock? Public Waterways, Road Cuts, Landscape Supply, Knap-Ins.
How to Cook It?  200° for 24hrs then 275° to 500° for 4hrs (depending on type), Cool for 12hr

Offline Pat B

  • Administrator
  • Member
  • Posts: 37,633
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #3 on: November 29, 2011, 08:07:37 pm »
Thanks Patrick. Cool info. Maybe we should add "pitch glue" to wikipedia.  ;D
Make the most of all that comes and the least of all that goes!    Pat Brennan  Brevard, NC

Offline JackCrafty

  • Global Moderator
  • Member
  • Posts: 5,628
  • Sorry Officer, I was just gathering "materials".
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #4 on: November 29, 2011, 11:01:49 pm »
Go for it Pat!
Any critter tastes good with enough butter on it.

Patrick Blank
Midland, Texas
Youtube: JackCrafty, Allergic Hobbit, Patrick Blank

Where's Rock? Public Waterways, Road Cuts, Landscape Supply, Knap-Ins.
How to Cook It?  200° for 24hrs then 275° to 500° for 4hrs (depending on type), Cool for 12hr

Offline mullet

  • Global Moderator
  • Member
  • Posts: 22,911
  • Eddie Parker
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #5 on: November 29, 2011, 11:21:12 pm »
It sure would have been easier, Patrick. I wonder if anybody still sells it?
Lakeland, Florida
 If you have to pull the trigger, is it really archery?

Offline JackCrafty

  • Global Moderator
  • Member
  • Posts: 5,628
  • Sorry Officer, I was just gathering "materials".
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #6 on: November 29, 2011, 11:40:52 pm »
I think there are some knife makers that sell it.  I saw that question on a knife maker forum and no one knew of any commercial outfit that sells the stuff in bulk... but several of those guys make up their own batches and have extra.
Any critter tastes good with enough butter on it.

Patrick Blank
Midland, Texas
Youtube: JackCrafty, Allergic Hobbit, Patrick Blank

Where's Rock? Public Waterways, Road Cuts, Landscape Supply, Knap-Ins.
How to Cook It?  200° for 24hrs then 275° to 500° for 4hrs (depending on type), Cool for 12hr

Offline mullet

  • Global Moderator
  • Member
  • Posts: 22,911
  • Eddie Parker
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #7 on: November 29, 2011, 11:46:33 pm »
Hmm,, same as we do. I'd buy bulk.
Lakeland, Florida
 If you have to pull the trigger, is it really archery?

Offline footfootfoot

  • Member
  • Posts: 107
  • Now with more irony
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #8 on: November 30, 2011, 01:05:54 am »
Awesome. Now I have a use for all that brick dust in my basement.
Bring me my Bow of burning gold; Bring me my Arrows of desire: Bring me my Spear: O clouds unfold! Bring me my Chariot of fire!

Offline sadiejane

  • Member
  • Posts: 1,030
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #9 on: December 01, 2011, 12:14:19 pm »
find the term "synthetic resin" interesting...
wild women don't get the blues

Offline jamie

  • Member
  • Posts: 2,387
  • born again pagan ,dirt worshipping heathen
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #10 on: December 07, 2011, 08:59:07 am »
used it this year doing some work with bob berg. stuff is amazing. you can buy it but it doesnt take much to make it
"Man is a tool-using animal. Without tools he is nothing, with tools he is all."

waterbury, ct

Offline half eye

  • Member
  • Posts: 3,300
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #11 on: December 07, 2011, 10:25:37 am »
Fellas,
     I make my own for mounting blades (including my arrow heads. Here is a couple of knives I just finished up
rich

Offline JackCrafty

  • Global Moderator
  • Member
  • Posts: 5,628
  • Sorry Officer, I was just gathering "materials".
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #12 on: December 07, 2011, 12:36:20 pm »
Jamie, where can you buy it?  Just curious.
Any critter tastes good with enough butter on it.

Patrick Blank
Midland, Texas
Youtube: JackCrafty, Allergic Hobbit, Patrick Blank

Where's Rock? Public Waterways, Road Cuts, Landscape Supply, Knap-Ins.
How to Cook It?  200° for 24hrs then 275° to 500° for 4hrs (depending on type), Cool for 12hr

Offline sadiejane

  • Member
  • Posts: 1,030
wild women don't get the blues

Offline JackCrafty

  • Global Moderator
  • Member
  • Posts: 5,628
  • Sorry Officer, I was just gathering "materials".
Re: Cutlers Resin - The Old Term for Pine Pitch Glue
« Reply #14 on: December 07, 2011, 02:50:44 pm »
Thanks Sadie!  I've got some of that stuff from them.  But that's not cutler's resin.  Brewers pitch is used to coat the inside of wooden or leather vessels that hold liquids.
Any critter tastes good with enough butter on it.

Patrick Blank
Midland, Texas
Youtube: JackCrafty, Allergic Hobbit, Patrick Blank

Where's Rock? Public Waterways, Road Cuts, Landscape Supply, Knap-Ins.
How to Cook It?  200° for 24hrs then 275° to 500° for 4hrs (depending on type), Cool for 12hr