Member
Posts: 29
Urac 185
«
on:
May 03, 2009, 12:37:28 am »
Hello,
I want to know if URAC 185 requires a heat source to cure and bond. I looked at the instruction sheet here
http://www.highlandwoodworking.com/library/urac.pdf
I found no declaration which states it needs a heat source greater than what appears to be 60-70 degrees F. The plan is to use URAC 185 on my next bow and I have either been building self bows or using Smooth On. However I would like to try URAC 185 and was also wondering if you have any gotchas, tips or recommendations which I might want to know about and cannot get from their instruction sheet. Is is worth using on the bow tips?
Thank you
Logged
>>>-------|>
Gordon
Member
Posts: 3,299
Re: Urac 185
«
Reply #1 on:
May 03, 2009, 03:18:12 am »
Urac does not require heat to cure, though it will cure quicker in warmer temps. For tips I use either 5 min epoxy or superglue.
Logged
Gordon
chep
Member
Posts: 29
Re: Urac 185
«
Reply #2 on:
May 03, 2009, 08:50:10 pm »
Do you need a smooth or rough gluing surface?
Logged
>>>-------|>
woodsrunner
Member
Posts: 73
Re: Urac 185
«
Reply #3 on:
May 04, 2009, 09:39:30 am »
Surface should be rough. I rough mine up with a toothing plane blade to give it more surface to adhere to. But an 80 grit sandpaper should work just a well.
Logged
Bowhunting is a passion, not an obsession. Its just hard for my wife to tell the difference sometimes.
Print
Pages: [
1
]
« previous
next »
Primitive Archer
»
Main Discussion Area
»
Bows
»
Urac 185