How do heat reflex in erc?  And does it require heat treating?  My stave is floor tillered and ready. I just need to know how to proceed. Thanks for any help
Freedom dies one compromise at a time. III%

Offline joachimM

  • Member
  • Posts: 675
  • Good - better - broken
Re: Heating erc?
« Reply #1 on: March 31, 2016, 02:37:39 pm »
Of nearly all woods ERC is most elastic in compression. For that reason I wouldn't temper it.

Offline Aaron H

  • Member
  • Posts: 3,437
Re: Heating erc?
« Reply #2 on: March 31, 2016, 02:40:57 pm »
I have had very good results with steam bending erc, I just sealed with shellac and steamed the same as I do my Osage, but I don't think it was necessary to steam that long (30 min. per 1/2").  Bent like butter.  Never tried tempering

Offline Springbuck

  • Member
  • Posts: 1,545
Re: Heating erc?
« Reply #3 on: April 07, 2016, 08:01:00 pm »
 I've bent it just slightly with steam and dry heat.  I don't think dry heat/tempering improves it much, like other woods.  It seemed barely effected, and if anything more brittle.